Milling. Polishing. Done.
cameo KrystaFree is a CAD/CAM block made of lithium glass ceramic with a nanoscale, interlocking microstructure. The block is already crystallised – no crystallisation or sintering is required. After milling, the restoration is simply polished and can be fitted straight away. A single crown can thus be milled in around 15 minutes.
The consistently stable marginal edge reduces microleakage and thus the risk of secondary caries. With a flexural strength of 380 MPa, KrystaFree is suitable for chairside and laboratory fabrication using the wet milling process, for example on the DGSHAPE DWX-43W.
| Material | Lithium glass ceramic, pre-crystallised |
| Flexural strength | 380 MPa |
| Coefficient of thermal expansion (25–500 °C) | 10.5 ± 0.5 × 10⁻⁶ K⁻¹ |
| Chemical solubility | < 40 µg/cm² |
| Density | 2.47 ± 0.05 g/cm³ |
| Translucency | ST – ultra-high (can be reduced by firing, if required) |
| Block size | 18 × 13 × 15 mm |
| Firing | not required – polishing is sufficient |
| Colours | A1, A2, A3, A3.5, B1, C1, D2, Bleach BL1, BL1, BL3 |
| Pack | 5 blocks per colour |
Indications: Veneers, inlays, onlays, partial crowns, and anterior and posterior crowns.
- No sintering or crystallisation firing; short fabrication time
- No shrinkage, no warping during glazing and firing
- Stable edges, no chipping during milling
- Good adhesive bonding, minimal wear on the antagonist tooth
Preparation: Shoulders rounded or bevelled on the inside, no sharp edges; allow approximately 1 mm of space at the incisal edge for finishing. For finishing, Aidite recommends the cameo KrystaFree polishing kit – unsuitable grinders may cause edge marks or overheating.
Firing is not necessary – polishing is sufficient. If you wish to stain or glaze, this can be done in a single firing, for example using Aidite Biomic Stain/Glaze. A crystallisation firing is also available for reduced translucency.
| Firing | Start | Heating | Final temperature / holding time | Open |
|---|---|---|---|---|
| Glaze/stain firing (example: Aidite kiln) | 450 °C | 55 °C/min | 730 °C / 1 min – max. 780 °C, otherwise translucency decreases | 600 °C |
| Crystallisation firing for reduced translucency | 450 °C, dry for 2 min | 50 °C/min | 840 °C / 3 mins | below 600 °C |
Etch the veneers with 4.5% hydrofluoric acid for 90–120 seconds prior to adhesive bonding. The full processing instructions can be found under Downloads.
Scan and design, wet milling, polish – no furnace required and no waiting time for the crystallisation firing.